1)
Materials: laminated wood
Density: 1.35 - 1.4 g/cm3
Thermal Conductivity1: 0.223 W/m*K(23 degreeC)
0.157 W/m*K(-165 degreeC)
2)
Materials: laminated wood
Density: 0.9 - 1.1 g/cm3
Thermal Conductivity1: 0.178 W/m*K(24 degreeC)
0.116 W/m*K(-165 degreeC)